Abstract
Medium-energy Ion Scattering Spectroscopy (MEISS) can provide non-destructive quantitative surface and near-surface composition with atomic layer depth resolution. The special features of MEISS can be utilized to improve quantification of conventional surface analysis techniques by studying preferential sputtering, which is one of the major problems in quantitative surface analysis using sputtering techniques. This phenomenon was studied in detail with MEISS, in situ and ex situ XPS analysis, RBS, and (inductively coupled plasma optical emission spectrometry) for WSi 2 .
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.