Abstract

Mechanical properties of high purity polycrystalline cBN sintered bodies synthesized by the direct conversion method under high pressure and high temperature have been investigated by hardness and transverse rupture strength (TRS) measurement in the temperature range of 20–1200 °C. It was confirmed that the hardness and TRS of the polycrystalline cBN depends strongly on the cBN grain size and the amount of residual (compressed) hBN in the sintered body. The fine-grained ( 99.9%) polycrystalline sintered body synthesized at 7.7 GPa, 2200–2400°C has highest hardness and TRS at any temperature. The TRS of the sintered body shows a positive temperature dependence up to 1200 °C. The high hardness and high TRS at high temperature of the fine-grained high purity polycrystalline cBN suggest that the sintered body has high potential in cutting tool uses.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.