Abstract

Clinical methods for heat treating composite resin restorations have been developed. In this investigation, the effect of heat treatments on the diametral tensile strength of composite resin was determined. The composite resin restorative materials were selected according to the manufacturers' suggested use for anterior or posterior teeth, filler particle composition, and light-cured or chemical polymerization. Samples were prepared according to American Dental Association specification No. 27, and heat treatments were accomplished with a Coltene DI 500 oven for curing at approximately 120 ° C for 7 minutes. Heat treatment substantially increased the diametral tensile strength tested, with the exception of the anterior hybrid particle ( p < 0.05). Composite resins with fine-particle inorganic fillers were significantly stronger than hybrid and microfilled composite resins.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.