Abstract

Titanium aluminide alloys offer considerable promise for use in high temperature applications, such as gas turbines. In this study an extruded Ti–46Al–5Nb–1W alloy has been examined, in terms of its tensile and creep behaviour. A reasonably fine and uniform microstructure was found in this bar product. This gave excellent properties, with tensile strengths up to ∼950 MPa at room temperature, along with 1% elongation. These properties were accompanied by a very good creep behaviour, with low primary strains at the lower stresses and very low secondary creep rates. Comparison of the creep properties of this titanium aluminide alloy with other similar compositions and some typical nickel alloys shows that it is significantly superior to first generation titanium aluminides but also nickel alloys, such as IN718 and Udimet 720Li. However, the strain controlled fatigue performance of the titanium aluminide alloy was significantly poorer than these same wrought nickel alloys.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.