Abstract

We measure the short circuit current improvement of various commercial backsheets for passivated emitter and rear solar cells (PERC) in photovoltaic (PV) modules. We quantify this improvement by a light recovery factor k defined as the share of the light reflected by the backsheet around the cell in a PV module laminate, which is converted into electrical current by the solar cells in the module relative to a reference rear surface. The presented measurement method allows measuring the light recovery factor as function of the incident light beam angle, which are important for the calculation of the yield analysis in the field. Simulations of the recovery factor with the optical ray tracing program DIADALOS are performed in order to support the interpretation of the results. For measuring the absolute light recovery probability of a backsheet one should use a reference backsheet with an absorbance of close to 100% to avoid systematic reflection errors especially for high incident light beam angles > 50°. The ranking of various recovery factors are compared to the ranking measured by reflectance measurements defined in standard IEC 62788-2 Ed.1 for backsheets. The standard shows a substantial deviation between the ranking of recovery factor and the reflectance which can be corrected by using an adapted definition for the reflectance measurement method.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.