Abstract
A crack manufacturing method is proposed for producing axial outer-diameter stress corrosion cracking (ODSCC) in Alloy 600 steam generator tube specimens. The process can be conducted at ambient conditions and, unlike conventional methods, it does not require complicated facilities. Eddy current testing and destructive examination data for the axial ODSCC specimens were compared with the available field crack data to determine whether those SCC specimens are representative in accordance with an existing industry guideline. Based on the results of our investigations, it was determined that the proposed method could be used to manufacture representative axial ODSCC in Alloy 600 tube specimens.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.