The surface of a Fe-Ni-Cr Alloy (SUS316L) plate was electrochemically nitrided in molten LiF-KF salt including Li3N at 873K. The crystal structure changed from fcc structure to bct structure with nitrogen introduction. The Nitrogen diffusion layers were predominately formed at nitrogen concentration of 23 at%. The nitriding process drastically also changed its magnetic property from non-magnetic to ferromagnetic. The magnetic field of 20 kOe saturated the magnetic moment with its magnetization of 81 emu/g at 10K. The anisotropic magnetization is ascertained. Based on CrN formation and Cr extraction from the original Fe-Ni-Cr system, the induced ferromagnetism was discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.