Abstract

Small volumes of Pd44Ni10Cu26P20 and Pd43.2Ni8.8Cu28P20 were encapsulated in B2O3 and thermally cycled between Tg−60°C and Tl+60°C, where Tg and Tl denote the alloys’ glass transition and liquidus temperatures. After this thermal treatment, the critical cooling rates (CCRs) for glass formation can be lowered by an order of magnitude, resulting in a critical cooling rate significantly lower than that reported for any other glass forming alloy melt. These experiments demonstrate that the CCR is not constant but strongly dependent on the degree of heterogeneous nucleation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.