Abstract

Areal density growth in longitudinal magnetic recording requires physical scaling of component features and properties that cannot continue indefinitely. The authors discuss in this paper the limitations and extendibility of longitudinal recording media focusing on its microstructural features and historical rate of change. Based on these trends, they estimate that an areal density of 200 Gb/in/sup 2/ is achievable. In order to make such media thermally stable, synthetic antiferromagnetic structures will likely be used. The crystallographic grain size will be between 5 and 6 nm and the coercivity of the media will likely not exceed 5000 Oe. Additionally, a significant decrease from current values in the width of the grain size distribution will need to occur to satisfy SNR requirements in the drive.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.