Abstract

ABSTRACTThe liquidus temperature (TL) often limits the loading of high-level waste in glass through the constraint that TL must be at least 100°C below the temperature at which the glass viscosity is 5 Pa-s. In this study, values of TL for spinel primary crystalline phase were measured as a function of glass composition. The test glasses were based on high-iron Hanford Site tank wastes. All studied glasses precipitated spinel (Ni,Fe,Mn)(Cr,Fe)2O4 as the primary crystalline phase. TL was increased by additions of Cr2O3, NiO, Al2O3, Fe2O3, MgO, and MnO; while Li2O, Na2O, B2O3, and SiO2 had a negative effect. Empirical mixture models were fitted to data.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.