Alumina preforms containing artificial pores were sintered at 1630°C in air and vacuum. Glass penetration into the alumina preforms was conducted at 1600°C in air. It was found that the trapped gases in alumina preforms sintered in air caused the random and incomplete filling of the smaller and larger artificial pores. In contrast, the pores in the alumina preform sintered in vacuum were completely filled during glass penetration.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.