Abstract

The performance of coir fiber in the production of linerboard made from soda-anthraquinone (soda-AQ) pulp was evaluated. Based on chemical analysis, the composition of coir fiber is suitable for the pulping process. Out of nine pulping conditions characterized, a pulping condition of 18% active alkali for 90 min cooking time was chosen. These conditions provided the highest screened yield (48.99%), a low rejection yield (0.27%), high viscosity (11.73 cP), and a kappa number (41) that is acceptable for unbleached linerboard production. Beating strengthened the coir pulp. Analyzing the beating revealed that coir pulp was optimized at 1000 to 2000 revolutions, based on a graph of freeness vs. burst index. For all beating conditions (1000 to 8000 revolutions), FESEM micrographs showed the presence of internal and external fibrillation of the fiber, which gradually increased fiber conformability and improved the inter-fiber bonding within the paper formation. Based on its burst strength of 4.57 kPa.m2/g and ring crush test of 1.76 Nm2/g, which complies with the minimum requirement of the industry standard, coir fiber can be considered an alternative fiber source for linerboard production.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.