The deactivation and regeneration of selective catalytic reduction (SCR) catalysts poisoned by potassium by a wet-impregnation method was investigated experimentally. Potassium in the form of both chloride and sulfate is a strong poison for the catalyst. The results indicate that potassium titrates the active sites for NH3 adsorption. Simply increasing the operating temperature or the vanadium content in the catalyst cannot compensate the loss of catalyst activity: Increasing the temperature hardly increases the conversion of NO for the strongly poisoned catalysts, and catalysts with high vanadium content become active for oxidizing NH3 to NO, causing a net NO formation. Deactivated catalysts can be regenerated by different methods. Sulfation by gaseous SO2 is efficient provided the poison is first removed by washing. When regenerating by 0.5 M H2SO4, the catalyst regains a higher activity than that of the fresh catalyst at temperatures higher than 300 °C. Heat treatment of the catalyst at 400 °C for 2 h...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.