Abstract

The leaching of cobalt from cobalt-bearing ternary sulfide with sulfuric acid solution under atmospheric pressure was investigated. The influence of stirring speed, leaching temperature, H2SO4 concentration, and particle size on the leaching efficiency of cobalt was studied, and the kinetics analysis of cobalt leaching from the cobalt-bearing ternary sulfide was performed. The results showed that cobalt and iron were selectively leached with high efficiency (>99%) under the optimal conditions, while molybdenum and copper were enriched in residues. According to the analysis of the experimental data, the leaching of cobalt conformed to the shrinking core model with a solid product layer and was controlled by internal diffusion. The activation energy of the leaching reaction was 49.86 kJ/mol, and the reaction orders of H2SO4 concentration and particle size were 0.57 and –1.4, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.