Abstract

Achiral poly(diphenylacetylene)s (PDPAs: pMe3, pEt3, piPr3, pMe2O1, pMe2OD1, and mMe3) with different alkyl side chains at the para or meta position of the side phenyl ring were prepared to examine achiral-to-chiral transformations upon thermal annealing in a chiral solvent. All the para-substituted PDPAs showed significant circular dichroism (CD) enhancement upon annealing, whereas the meta-substituted polymer, mMe3, was inert to the same treatment. To investigate the kinetics, the asymmetric conformational change was monitored by observing the changes in the magnitude of circular polarization (gCD) or optical rotation. PDPAs with bulkier, round-shaped side groups (pEt3 and piPr3) had greater gCD values at equilibrium than pMe3 with a smaller side group. Moreover, the activation energy for the forward reaction (Eaf) was lower in the bulkier polymers than in pMe3 owing to enhanced miscibility with the chiral solvent. Similarly, the long alkyl chains of pMe2O1 and pMe2OD1 acted as internal plasticizers to ...

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.