Abstract
The ion conduction of yttria-stabilized zirconia (YSZ) was studied by varying the doping ratios during atomic layer deposition (ALD). The ALD cycle ratio for the yttria and zirconia depositions was varied from 1:1 to 1:6, which corresponded to the doping ratios from 28.8% to 4.3%. The in-plane conductivity of ALD YSZ was enhanced by up to 2 orders of magnitude; the optimal ALD doping ratio (10.4%) was found to differ from that of bulk YSZ (8%). This different relationship between the doping ratio and the ion conduction for ALD YSZ versus bulk YSZ is due to the inhomogeneous doping in the vertical direction of the ALD YSZ films, as opposed to the homogenous doping of bulk YSZ.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.