Abstract

Abstract Selective corrosion in a hot hydrochloric acid service was noted in a narrow band of the heat affected zone of a commercially fabricated zirconium weldment. Little attack was present on the weld proper or the parent stock. The selective attack has been found to be intergranular in nature and associated with the presence of a precipitated phase in the grain boundaries. The particular precipitated phase required for this attack has been duplicated in bulk samples by specific heat treatment, as well as in experimental weldments. Two methods of prevention of this localized attack near welds have been evaluated; namely: (1) Use of high purity zirconium, and (2) heating of commercially pure zirconium weldment at 1800 F followed by a water quench. Possible mechanisms for the microstructural changes and for the corrosion attack are discussed. 6.3.20, 3.2.2, 4.3.2, 3.7.3

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.