The possible stages of interaction between glass and film-forming solutions are considered. The effect of the amounts of acid and water in solution of the destruction of glass is demonstrated. An analysis of the relationship between the quantities of Na2O and SiO2 and the transition-layer width is provided.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.