The research work reported in this paper is an investigation of the behavior of barium titanate powders under selective laser irradiation. Our goal is to determine suitable conditions to sinter the powders and form dense layers usable in some electronic components. On that purpose, compacts of micro/nano BaTiO 3 powder mixes are used for a parametric investigation of the laser scans parameters (power, speed, etc.) with a Nd-YVO 4 laser (23 W). The microstructures obtained after laser treatments are evaluated by XRD, SEM and EDS and compared to a reference specimen manufactured in a conventional way. From this work it can be concluded that a high laser beam power is required to obtain a consolidation of the powder grains and the use of a high scan speed avoids the melting. The scanning speed also influences the final crystallographic state of BaTiO 3 . Optimal parameters were founded in order to form a dense and homogeneous tetragonal BaTiO 3 surface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.