Abstract
The corrosion behavior of stainless steel samples (304L and 316L) in HCl and H2SO4 solution has been studied using potentiodynamic, cyclic voltammogram, EDX and scanning electron microscope (SEM) techniques. The inhibition characteristics of 2-mercaptobenzoxazole (MBO) on 316L stainless steel (316L SS) in HCl solutions were investigated at different temperatures (25, 40, 50 and 60°C). MBO compound has proven to be efficient inhibitors for general and pitting corrosion of 316L SS in HCl solution. The inhibitive property of MBO may be argued to the formation of very low soluble bis-benzoxazolyl disulfide (BBOD) layer and a compact Fe–MBO complex film on the electrode surface. Some samples were examined by scanning electron microscope. The inhibition efficiencies increased with the increasing of MBO concentration but decreased with increasing temperature. The activation energy and thermodynamic parameters were calculated.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.