FeCrNi alloy after aluminizing was oxidized at 1000 °C in dry and humid (2.23 vol.% water) H 2. Experimental results showed that H 2 promotes the formation of θ alumina and its transformation to α alumina. The morphology of surface alumina coating does not change significantly, but the oxidation rate of the aluminized layer accelerates by the addition of water vapor. As a result, more cracks are found beneath the alumina layer when water vapor is present. The addition of water vapor seems having a favorable effect on the selective oxidation of Al and concentration of oxygen vacancy in the aluminized alloys.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.