Abstract

The effect of roman PH 2 O and flow rate on the oxidation of 304Lat 873 K in oxygen is reported. High concentrations of water vapor and highflow rates result in breakaway corrosion. The mass gain after 168 hrincreased by four to five times, compared to oxidation in dry O2. Inthe presence of H2O, the corrosion products consisted of arelatively thin (Cr,Fe)2O3 oxide plus large oxide islandsconsisting mainly of Fe2O3. A mechanism explaining theeffect of water vapor on marginal chromia formers is proposed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.