Abstract
Titanium is a key element in nickel-base superalloys needed with aluminum to achieve the desired volume fraction of the strengthening γ′-phase. However, depending upon its concentration, titanium can degrade the adherence of aluminum oxide by forming TiO2 particles near the oxide-metal interface. This effect is extended to thermal barrier coating systems where in this case, the bond coat replaces the superalloy as the underlying substrate. Noting that the onset of failure of thermal barrier coating systems coincides with the first spall of the thermally grown oxide, titanium level in the superalloy can have an important effect on the useful life of the coating. Therefore, this study was undertaken to examine the effect of titanium on the performance of a thermal barrier coating system. Included in the study were two Ni-base superalloys with similar chemical composition except for the Ti content and a Pt-containing bond coat consisting of γ′+γ-phases all top coated with zirconia stabilized by 7 wt % yttria. Coating performance was evaluated from thermal exposure tests at 1150°C with a 24 h cycling period to room temperature. Various electron-optical techniques were used to characterize the microstructure. The coating system on the low-Ti alloy was found to outperform that on the high-Ti alloy. However, for both alloys, failure was observed to occur by loss of adhesion between the thermally grown oxide and underlying bond coat.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.