Prior investigation suggested that a temperature-induced liquid–liquid structure transition (TI-LLST) could occur in Sn–Bi40wt-% alloy around 879°C. Based on the results of TI-LLST, the Sn–Bi40wt-% alloys are melted and held at the temperature above and below TI-LLST, respectively, and then solidified from the same temperature. The aim of this work was to explore the influence of TI-LLST on directional solidification microstructure by using the Bridgman method. The results show that dendritic arm spacing decreases and the microstructure is refined markedly for the samples solidified from the melt which experienced the TI-LLST.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.