The ferromagnetic Li 0 . l0 CU 0 . lO Nio. 30 Zno. 4o Fe 2.1 O 4 synthesized by the typical ceramic technique which is sintered at the various temperatures. The formation of single phase cubic spinel structure at varied sintering temperatures (T s ) is confirmed by the x-ray diffraction (XRD) analysis. XRD pattern confirms that the T s does not distress the inner structure of the sample. The bulk density and theoretical density are found to be improved with T s . Due to increasing of T s, a normal fast grain growth happens over the pores volume which reduced the porosity with sample density. The value of relative quality factor (RQF) and initial permeability are also enhanced with T s because of low porosity and high density. The peaks of the relative quality factor are shifted toward to the left with the T s which indicates the decreasing trend of the loss factor. The characteristics of structural, density, porosity, relative quality factor, initial permeability and loss factor of the composition are explained here.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.