Root cause and possible processing remediation of tablet capping were investigated using a specially designed tablet press with an air compensator installed above the precompression roll to limit compression force and allow extended dwell time in the precompression event. Using acetaminophen-starch (77.9:22.1) as a model formulation, tablets were prepared by various combinations of precompression and main compression forces, set precompression thickness, and turret speed. The rate of force application (RFA) was the main factor contributing to the tablet mechanical strength and capping. When target force above the force required for strong interparticulate bond formation, the resultant high RFA contributed to more pronounced air entrapment, uneven force distribution, and consequently, stratified densification in compact together with high viscoelastic recovery. These factors collectively had contributed to the tablet capping. As extended dwell time assisted particle rearrangement and air escape, a denser and more homogenous packing in the die could be achieved. This occurred during the extended dwell time when a low precompression force was applied, followed by application of main compression force for strong interparticulate bond formation that was the most beneficial option to solve capping problem.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.