The influence of glass coating thickness on the interfacial heat transfer coefficient has been examined using numerical modeling. Temperature and heat flux during working of a Inconel 718 work-piece and colder H13 dies have been simulated. The thickness of the glass coating is found to have a significant influence on the forming characteristic.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.