This study evaluates the effects of gamma radiation on structure, electrochemical corrosion behavior and Vickers hardness of commercial dental Nikkeli–Kromi–Polttosekoitus [Ni65.2Cr22.5Mo9.5X2.8 (X=Nb, Si, Fe and Mn)] alloy. The corrosion rate of Ni65.2Cr22.5Mo9.5X2.8 (X=Nb, Si, Fe and Mn) alloy with 0.5 M HCl is increased with increasing the exposure rate of gamma radiation. The corrosion resistance of Ni65.2Cr22.5Mo9.5X2.8 (X=Nb, Si, Fe and Mn) is varied and reaches a minimum value at 30 KGy. The corrosion potential value also is varied and reaches its highest value at 30 KGy. The Vickers hardness value of Ni65.2Cr22.5Mo9.5X2.8 (X=Nb, Si, Fe and Mn) alloy is decreased by increasing the gamma radiation dose. Also it is obvious from our results that the effects of gamma radiation at the surface are much higher as compared with deeper parts and the structure of the alloy is changed due to its exposure to gamma radiation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.