Abstract

The corrosion behavior of the as-received steel and the spheroidized steel in acidic chloride environment was investigated. The results indicate the corrosion mode and corrosion rate of two steels are diverse due to their difference in microstructure. For as-received steel with ferrite-pearlite microstructure, severe localized corrosion happens on the pearlite regions, and plenty of cathodic cementite remains in the pits, further strengthening the micro-galvanic effect and accelerating the corrosion rate. While for spheroidized steel with tempered martensite microstructure, the nanosized cementite particles evenly distributed on the ferrite substrate are easy to fall off, which can significantly reduce the cementite accumulation on the steel surface, relieving the acceleration effect of micro-galvanic corrosion.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.