Abstract

Cold flakes, one of casting defects, were observed through acoustic microscopy in aluminum alloy die-cast plates (ADC12), and specimens having a cold flake of different sizes were prepared and subjected to the tensile testing. The tensile strength linearly decreased with the size of the cold flake, and the decreasing rate of the strength was greater for the specimen with the exposed cold flake than that with the embedded cold flake. The in-process ultrasonic measurement was carried out during tensile testing, and it was found that the oxide layer of the cold flake was

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.