Abstract

Addition of electrolyte additives (ethylene or vinylene carbonate) is shown to dramatically improve the cycling stability and capacity retention (1600 mAh g-1) of Si nanowires (NWs) in a safe ionic liquid (IL) electrolyte (0.1LiTFSI-0.6PYR13FSI-0.3PYR13TFSI). We show, using postmortem SEM and TEM, a distinct difference in morphologies of the active material after cycling in the presence or absence of the additives. The difference in performance is shown by postmortem XPS analysis to arise from a notable increase in irreversible silicate formation in the absence of the carbonate additives. The composition of the solid electrolyte interphase (SEI) formed at the active material surface was further analyzed using XPS as a function of the IL components revealing that the SEI was primarily made up of N-, F-, and S-containing compounds from the degradation of the TFSI and FSI anions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.