Abstract

In a previous study, the authors developed Nd–Fe–B/glass two-layer films deposited on Si substrates using pulsed laser deposition for micro electro mechanical systems. Here, the fabrication conditions of the films were investigated to determine the optimum conditions that enhance the magnetic properties of the films. The annealing time in the pulse-annealing process conducted after the deposition was set to 4.0 s at Nd contents of 14 at.–16 at.%. Moreover, the effect of the glass/Nd–Fe–B thickness ratio on the magnetic properties was examined. A ratio less than 2 resulted in an increase in (BH)max up to 80 kJ/m3.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.