To improve the anti-oxidation properties of carbon fibers (CFs), the sol-gel method followed by pyrolysis was used to coat CFs with SiC/SiO2 ceramic coatings. The SiO2 sol-gel coating was performed by dip coating a PAN(polyacrylonitrile)-based stabilized fiber (PSF) in a silica sol prepared by the polycondensation of tetraethylorthosilicate (TEOS) in the presence of an acidic catalyst. The PSF coated with SiO2 sol then underwent heat treatments at high temperatures in an inert atmosphere to deposit the SiC/SiO2 and carbonize the deposited fibers. The surface morphology of the CFs deposited with SiC/SiO2 was characterized using a scanning electron microscope (SEM). The relative oxidation resistance of the SiC/SiO2 layer deposited on the CFs was determined by the weight loss due to the use of a thermogravimetric analyzer (TGA) under flowing air, and the data were used to calculate the activation energies through an Arrhenius plot.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.