Abstract

Zero-valent iron (ZVI) and green rusts can be used as reductants to convert chromium from soluble, highly toxic Cr(VI) to insoluble Cr(III). This study compared the reduction rates of Cr(VI) by ZVI and two carbonate green rust phases in alkaline/hyperalkaline solutions. Batch experiments were carried out with synthetic chromate solutions at pH 7.7–12.3 and a chromite ore processing residue (COPR) leachate (pH ≈ 12.2). Green rust removes chromate from high pH solutions (pH 10–12.5) very rapidly (<400 s). Chromate reduction rates for both green rust phases were consistently higher than for ZVI throughout the pH range studied; the surface area normalized rate constants were two orders of magnitude higher in the COPR leachate solution at pH 12.2. The performances of both green rusts were unaffected by changes in pH. In contrast, ZVI exhibited a marked decline in reduction rate with increasing pH to become almost ineffective above pH12.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.