This short communication pertains to the synthesis of heterogenite (HCoO2) and its reduction to submicron cobalt metal powder. Heterogenite was prepared from a commercially produced wet cobalt hydroxide, Co(OH)3, which was dried at 110°C to make heterogenite. HCoO2 thus prepared had 24% higher bulk density than mixed valance cobalt oxide, Co3O4 (CoOCo2O3). The reduction of heterogenite in hydrogen was studied via a design-of-experiment approach. The effect of three parameters i.e. time of reduction, temperature of reduction and hydrogen flow rate was studied on the reduction of heterogenite to cobalt metal powders of submicron sizes. The main advantage of using HCoO2 containing about 63% Co as feed for making cobalt metal powder will be the higher productivity and capability of making different sizes of cobalt metal powders such as sub-micron, half-micron and extra-fine.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.