Abstract

It is known that advanced and ultra-high strength steel grades (AHSS and UHSS) are susceptible to hydrogen embrittlement under certain test conditions [1, 2]. In this study, punched hole specimens for constant load testing with in situ hydrogen charging were used to quantify the effect of different corrosive conditions. Flowing or stagnant electrolyte (5% NaCl) conditions were established and time to failure was recorded as a function of applied tensile stress. The pH of the solution was set at 2, 7, and 12. Bare and zinc-galvanized (EG) specimens were used. Hydrogen uptake as a function of immersion time was characterized.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.