PEO (Polyethylene Oxide) addition in chitosan has been successfully fabricated as a humidity sensor. In this study, 3% w/v chitosan solution was added by 0.1, 0.2, 0.3, 0.4 and 0.5 (%w/v) of PEO respectively. The sensing properties of chitosan and chitosan/PEO films as humidity sensors have been characterized using Air Handling Unit Trainer, model KT-2000AHU to determine response, repeatability, and recovery toward relative humidity (20-90% RH). The results show that the chitosan/PEO films have a good response when exposed to 90 %RH at room temperature. Those are 288,09 mV obtained by pure chitosan film; 338.97, 384.44, 406.81, 359.69, and 345.84 mV for 0.1, 0.2, 0.3, 0.4, and 0.5% of PEO films respectively that show higher electrical response. The smooth and porous film morphology and chemical interaction between chitosan and PEO through hydrogen bond obtained by SEM and FTIR could be responsible for the higher electrical response. Furthermore, humidity sensing material based on chitosan/PEO films shows good recovery and repeatability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.