Abstract

Hollow Y zeolite single crystals have been obtained from a conventional NaY zeolite following a three-step process involving a severe dealumination of the zeolite with silicon tetrachloride (step #1), followed by an acid washing under mild conditions (step #2) and finally a selective dissolution of the crystals core in the presence of protective Al species (step #3). Crystals are characterized by the presence of a regular internal cavity with 0.1–0.2 nm thick microporous walls. They contain a relatively low framework Al content but significant amounts of extraframework Al oxide species mainly located on the external surface of the crystals. Hollow crystals have been mixed with a Pt-supported alumina binder and used as catalysts in the hydroisomerization of n-hexadecane. Compared to the corresponding bulk crystals obtained after step #2, their higher activity has been attributed to a better efficiency, directly resulting from the presence of the cavity.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.