We report the fabrication and characteristics of a ZnO thin-film transistor (TFT) using a 50 nm thick ZnO film as an active layer on an Al2O3 gate dielectric film deposited by atomic layer deposition. Lowering the deposition temperature allowed the control of the carrier concentration of the active channel layer (ZnO film) in the TFT device. The ZnO TFT fabricated at 110 °C exhibited high-performance TFT characteristics including a saturation field-effect mobility of 11.86 cm2 V−1 s−1, an on-to-off current ratio of 3.09 × 107 and a sub-threshold gate-voltage swing of 0.72 V decade−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.