The high temperature response in torsion and creep of two extruded Mg-Zn alloys was investigated in the present study. The alloy 0 (Mg-2Zn-1Mn) was found to exhibit a lower strength than the alloy 2 (Mg-0.55Zn-0.79Mn-0.75Al-0.17Ca), even if the activation energy for creep was similar for both materials (170-180 kJ/mol). The difference in flow stress was here preliminarily attributed to the precipitation of fine Al2Ca particles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.