Abstract

LIGHT-WEIGHT calcium silicate hydrate (unit weight about 70 lb./ft.3) is made by curing cast mixtures of hydrated lime and silica for a number of hours in saturated steam at high temperatures. In previous work by Taylor and Moorehead1, it was shown that the maximum compressive strength for cast specimens depends on the lime–silica ratio and the specific surface area of silica flour used. A maximum compressive strength of 3,850 lb./in.2 at one day was achieved at a unit weight of 64 lb./ft.3 (strength/weight ratio 60) for specimens cured for 10 h in saturated steam at 186° C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.