Abstract

The aim of this investigation was to discuss the mechanical properties and aging-resistance of 3Y-TZP (3 mol% yttria-tetragonal zirconia with 0–0.25 wt% alumina added 3Y-TZP) by comparing the effect of high-energy ball milling zirconia powders (HP) and commercially available zirconia powders (CP). The results showed that a hardness of 12.93 GPa, combined with an excellent high-fracture toughness of 9.17 MPa m1/2, could be attained for HP-doped (0–0.25 wt% (Al2O3)) ceramics, as well as an increase in hydrothermal stability with the increase in Al2O3 content. The HP + 0.15 wt% (Al2O3) ceramics exhibited better antiaging performance and mechanical properties. These 3Y-TZP ceramics, with high-fracture toughness and better aging-resistance, which were prepared by a high-energy ball milling method, could meet the different demands of practical dental ceramics.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.