Abstract

This work evaluated the efficiency and systemic application of heterogeneous photocatalytic degradation for dairy wastewater under advanced oxidation process (AOP) utilizing solar radiation and immobilized ZnO as measured by total organic carbon (TOC). The AOP system consisted of a semibatch reactor and glass tank operated with an initial volume of 3 L of dairy wastewater. ZnO was immobilized on a metal plate of mm and used as a catalyst bed. Evaporation rate was considered when effective degradation of the photocatalytic system was determined. The AOP utilized Taguchi’s L8 orthogonal array. The entry variables were pH, reaction time, initial organic load in the effluent, and ZnO coating thickness on the catalyst bed. When optimized, an effective TOC degradation of 14.23% was obtained under variable values of pH 8.0, a metal-plate coating of 100 micrometers (μm) ZnO, and total reaction time of 180 min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.