Abstract
The high mechanical quality factor (Qm) of KNN-based ceramics is usually achieved by acceptor doping. However, this hardening effect has serious limitations due to the increased mobility of oxygen vacancies under large electric fields and hence is difficult to use in high-power applications. In this work, the hardening mechanism is demonstrated by the development composites of the 0.957(K0.48Na0.52)Nb0.94Ta0.06O3-0.04(Bi0.5Na0.5)ZrO3-0.003BiFeO3 (KNNT-BNZ-BFO) matrix with the K4CuNb8O23 (KCN) phase using the two-step ball-milling method. A decrease in remnant polarization and dielectric constant and an increase in resistivity and Qm are observed compared to that in the KNNT-BNZ-BFO sample. A high Qm of 160, Curie temperature, TC, of 310 °C, and piezoelectric coefficient, d33, of 330 pC/N can be obtained simultaneously in the composite with a 0.008 mole ratio of KCN. This can be explained by the mechanical clamping effect of KCN due to strain incompatibility and the domain wall pegging that traps charges at the KNNT-BNZ-BFO/KCN interface. This composite approach is considered a general hardening concept and can be extended to other KNN-based ceramic systems.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.