Abstract

Eu 2+-doped BaSi 2O 5 film phosphors on quartz substrates are fabricated by radio-frequency magnetron sputtering thermal diffusion. The BaSi 2O 5: Eu 2+ phosphor crystals have some preferred orientations that are lattice-spacing matched with the crystallized β - SiO 2 crystals, and they show pore and grain boundary-free morphology with a rod-like shape fused into the crystallized β - SiO 2 crystals. The BaSi 2O 5: Eu 2+ film phosphor has a high transparency, with a transmittance of about 30% in visible light. The BaSi 2O 5: Eu 2+ film phosphor shows 510 nm green emission from the f–d transition of the Eu 2+ ions, and in particular the best sample shows a green photoluminescence brightness of about 5% of a BaSi 2O 5: Eu 2+ powder phosphor screen. These excellences in optical properties can be explained by less optical scattering at pores or grain boundaries, and less reflection at the continuously index-changed interface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.