Up-conversion luminescence of Er3+-doped oxyfluoride germanate optical fiber is observed under laser-diode excitation. The enhanced green emission line is due to 2H11/2,4S3/2 → 4I15/2 transition of Er3+. The integrated luminescence intensity related to 2H11/2,4S3/2 → 4I15/2 (green) and 4F9/2 → 4I15/2 (red) transitions of Er3+ is reduced with increasing temperature. Several spectroscopic parameters of Er3+ ions in optical fibers were determined. The spectral linewidth is reduced, whereas the maximum of emission peak is shifted to longer wavelengths with increasing fiber length.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.