Abstract

We report a comparative frozen polarization study in three piezoelectric polymers: one polyimide without –CN dipolar groups (poly0CN), and two more that differ in the position of the –CN dipolar group present in the repetition unit (poly2-4 and poly2-6). The values of the dielectric permittivity and frozen polarization show that the participation of N-phenylphthalyimide group depends strongly on the curing process. For totally cured samples this group has little influence on the value of remnant polarization. The study was performed by dielectric measurements and by Thermally Stimulated Depolarization Current (TSDC) technique.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.