Abstract

Magnesia-Hercynite bricks destined for thermal shock applications in cement rotary kilns often show an enhanced crack propagation resistance due to an engineered microstructure design. In these materials, microcrack networks, resulting from the thermal expansion mismatch between magnesia matrix and Hercynite aggregates, promote the activation of energy dissipating mechanisms within the so-called Fracture Process Zone (FPZ) during loading. In this research, the fracture behaviour of a Magnesia-Hercynite material has been investigated by coupling an enhanced Digital Image Correlation method (2P-DIC) with the Wedge Splitting Test (WST). The coupling of these advanced characterisation methods is very effective in measuring important fracture parameters accurately and in highlighting characteristic fracture mechanisms, such as crack-branching. A refined R-curve approach is proposed with effective fracture energy calculations based on 2P-DIC measurements. The results demonstrate interesting correlations between FPZ development and an enhanced crack propagation resistance.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.