Abstract
AbstractThe present work is concerned with Er-doped oxidized porous silicon (PS). The characteristic feature of the work is that PS doping has been realized by an electrochemical procedure followed by a high temperature treatment. 5-μm thick PS layers were formed on p-type Si of 0.3-Ohm-cm resistivity. Er incorporation was performed by a cathodic polarization of PS in a 0.1 M Er(NO3)3 aqueous solution. A high temperature treatment in an oxidizing ambient at 500-1000°C was utilized to provide either partial or total oxidation of PS:Er layers. X-ray microanalysis was used to study chemical composition of the samples. Photoluminescence (PL) and photoluminescence excitation (PLE) spectra were investigated. After the partial oxidation (in the temperature range of 600-800°C), weak Er3+-related PL at 1.53 ptm was observed. A high temperature anneal in Ar atmosphere at the temperature of 1100°C caused a significant increase in the Er3+-related PL intensity. Resonant features were observed in PLE spectra of fully oxidized PS. Five peaks at 381, 492, 523, 654 and 980 nm were revealed. The strongest excitation occurred at 381 and 523 nm. The excitation of different Er3+ energy levels, cross-relaxation interactions and emission due to the 4I13/2→4I15/2 transitions were considered. Application of the Er-doped oxidized PS for integrated optical waveguides is presented.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.