Abstract
The effectiveness of three different designs of conduit plates was verified for even distribution of precursors in a voluminous forced-flow atomic layer deposition (ALD) chamber designed to hold macroscopic elongated substrates vertically. Furthermore, a new "soak function" was introduced in the controlling software of the ALD instrument. This function enabled increase in residence time of the precursor in the chamber without escalating the dosage. The flow of precursors guided by the conduit plates with and without application of the soak function was simulated using computational fluid dynamics. A conformal coating of TiO2 with good uniformity on Si and porous polysulfone fibers was achieved to evidence the design and efficacy of conduit plates and soak function.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.